Verified public resource

TITANIUM - Color Mark (20W) Laser Settings - Fiber 20W

A checked-in starting recipe for TITANIUM - Color Mark (20W) on Fiber 20W. Laser, lens, focus, coating, and material batches vary, so test this recipe on matching scrap before production.

Specifications and context

Laser source
Fiber (MOPA)
Model
Fiber 20W
Power
34%
Speed
750 mm/s
Frequency
45 kHz
Passes
1
Hatch interval
0.025 mm
Pulse width
Not specified

Production guidance

Use these parameters as a documented starting point, not a universal prescription. Material batches, optics, focus, air assist, source age, and machine calibration all affect the finished result. Confirm focus, protect the work area, and run a small test on matching scrap before committing a production piece. Record the date, material supplier, lens, focus method, and final parameter changes with the saved job so the result can be reproduced instead of rediscovered.

  1. 1. Oxide color marking on titanium. Adjust speed/power for different colors.
  2. 2. Run a small material test first, confirm focus and lens, then change one variable at a time.
  3. 3. Record the successful result in the Parameters Library so the next production run is repeatable.

Privacy Policy| Terms and Refund Policy| Contact and Support